Ultrasonic Testing Low Quality
Loading...
5,994
Loading...
Uploader Comments (sachithrupasinghe)
see all
All Comments (4)
-
excellent work dude.it was very helpful.but found it difficult to view the screen..it would be more helpful if u correct the problems in this vdo & post a new one..anyway thank u very much
-
@ 1:35 you said for example you like to test a 40 mm thick (carbon steel), you would calibrate the range to 50 mm?. In UT test 2 or more backwall echo must be shown, better calibrate it to 100 mm.
Loading...
thanks for the comment,
although i have uploaded this video , my knowledge about this test is still limited.
i will contact the instructor and give you an answer.
thankyou
sachithrupasinghe 1 year ago