Have you tried smaller 316L stainless steel plates (or washers) sanded in a crosshatch pattern as electrodes? spaced about 2mm or less submerged into distilled water with a little potassium hydroxide. Using different set ups with neutral plates? No contaminants then. I really wonder how that will perform... looking forward to the next video on this.
-
You could go to the dump and get a stainless steel sink for your electrodes. Also you could space your plates alot closer so then you dont need much salt and it works very good when you do that.
-
probably the reason the platinum coating didnt hold up is either because of contamination or those tiny little scratches you leave behind after holding them. in your video here you showed us a scratched platter. you could see the scratches in the reflection of the sunlight. they must be clean and unhandled and THEN, theyll work ;)
-
hello this is damn ==
-
those "1" and "0" must be screaming :D
-
good way to get the exp metals .
-
This video.. cool. See my home energy stuffif you like WIND POWER. Merry Christmas Y'ol!
-
coud i pull the platinum off of thees and on to jewlry using electro plating
-
Put a little bit of Naval Jelly (phosphoric acid) into your water and the platinum should "HEAL BACK" when it's not in use, corroding when in use, only.
-
The recombining hydrogen and oxygen into water and diagrams are for what I call Krell technology, the HHO SOLAR conversion is about ten stories high and is more like municipal oil or nuclear MUNICIPAL GENERATORS.