HVOF Is Better Than Chrome Plating
Loading...
3,457
Loading...
Uploader Comments (AtlasMachineTV)
see all
All Comments (8)
-
"Bright chromium deposits from conventional baths have a Vickers hardness of 900 to 1000" - New Hampshire Materials Laboratory
"Tungsten carbide is high melting, 2870 °C (5200 °F), extremely hard (8.5–9.0 Mohs scale, Vickers hardness number = 2242)" - Wikipedia, Tungsten Carbide
"Aluminum Titanium Nitride (AlTiN) is the hardest of the Physical Vapor Deposition (“PVD”) hard coatings at over 3500 Vickers" - Chemical Supermarket
-
@AtlasMachineTV for industrial use longevity is definitely the preferred option but i still say it dosent replace chrome
Loading...
After it has been ground and polished it will have a much longer life than chrome.
sanderg72 3 months ago
@sanderg72 Give us a call and we will answer any questions you have 855-GO-ATLAS
AtlasMachineTV 3 months ago
wait this is alternative to chrome?? ITS NOT EVEN SHINY!! hows that better then chrome??
citydriver 3 months ago
@citydriver It gives it WAY more service life, it will enhance the life of equipment for much longer and save a ton of money
AtlasMachineTV 3 months ago
@AtlasMachineTV well i understand that but saying is replaces chrome is wrong sins the surface isent shiny
citydriver 3 months ago
@citydriver its a much more cost effective option. would u rather a part be shiny or last five times longer?
AtlasMachineTV 3 months ago