Metal Spinning
Loading...
7,916
Loading...
Uploader Comments (zapzap112)
see all
All Comments (5)
-
I tried that with cartridge brass. I had to anneal it every two second it seems. It never did turn out right. Being I'm a novice, I've been working with 1100 and 3003 aluminum with great results. This is quite a unique craft that a lot of people aren't even aware of.
-
what is the the thickness of the copper sheet please ?
-
I think you've done that once before LOL Thanks for sharing. I'll have to give it a spin:o)
Loading...
It was only annealed once before spinning?
kenrinc 1 year ago
@kenrinc with the plate type being used is annealing is not necessary
zapzap112 1 year ago